Os motores de busca de Datasheet de Componentes eletrônicos
  Portuguese  ▼
ALLDATASHEETPT.COM

X  

23-21B/BHC-AN1P2/2A Folha de dados(PDF) 9 Page - HK TO-GRACE TECHNOLOGY CO.,LTD.

Nome de Peças 23-21B/BHC-AN1P2/2A
Descrição Electrónicos  Reverse Package Chip LED
PDF  10 Pages
Scroll/Zoom Zoom In 100%  Zoom Out
Fabricante Electrônico  TO-GRACE [HK TO-GRACE TECHNOLOGY CO.,LTD.]
Página de início  http://www.to-grace.com/index.html
Logo TO-GRACE - HK TO-GRACE TECHNOLOGY CO.,LTD.

23-21B/BHC-AN1P2/2A Folha de dados(HTML) 9 Page - HK TO-GRACE TECHNOLOGY CO.,LTD.

Back Button 23-21B/BHC-AN1P2/2A Datasheet HTML 2Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 3Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 4Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 5Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 6Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 7Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 8Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 9Page - HK TO-GRACE TECHNOLOGY CO.,LTD. 23-21B/BHC-AN1P2/2A Datasheet HTML 10Page - HK TO-GRACE TECHNOLOGY CO.,LTD.  
Zoom Inzoom in Zoom Outzoom out
 9 / 10 page
background image
EVERLIGHT ELECTRONICS CO.,LTD.
23-21B/BHC-AN1P2/2A
Everlight Electronics Co., Ltd.
http://www.everlight.com
Rev.1.0
Page: 9 of 10
Device No. : DSE-23B-B02
Prepared date: 08-08-2004
Prepared by: Jeff Tsai
Precautions For Use
1. Over-current-proof
Customer must apply resistors for protection , otherwise slight voltage shift will cause big
current change ( Burn out will happen ).
2. Storage
2.1 Do not open moisture proof bag before the products are ready to use.
2.2 Before opening the package, the LEDs should be kept at 30℃ or less and 90%RH or less.
2.3 The LEDs should be used within a year.
2.4 After opening the package, the LEDs should be kept at 30℃ or less and 70%RH or less.
2.5 The LEDs should be used within 168 hours (7 days) after opening the package.
2.6 If the moisture absorbent material (silica gel) has faded away or the LEDs have exceeded the
storage time, baking treatment should be performed using the following conditions.
Baking treatment : 60±5℃ for 24 hours.
3. Soldering Condition
3.1 Pb-free solder temperature profile
3.2 Reflow soldering should not be done more than two times.
3.3 When soldering, do not put stress on the LEDs during heating.
3.4 After soldering, do not warp the circuit board.
4. Soldering Iron
Each terminal is to go to the tip of soldering iron temperature less than 280℃ for 3 seconds
within once in less than the soldering iron capacity 25W. Leave two seconds and more intervals, and do
soldering of each terminal. Be careful because the damage of the product is often started at the time of the
hand solder.



Html Pages

1 2 3 4 5 6 7 8 9 10


Folha de dados Download

Go To PDF Page


Ligação URL



ALLDATASHEET é útil para você?  [ DONATE ] 

Sobre Alldatasheet   |   Publicidade   |   Contato conosco   |   Privacy Policy   |   Link para a ficha técnica    |   roca de Link   |   Lista de Fabricantes
All Rights Reserved©Alldatasheet.com


Mirror Sites
English : Alldatasheet.com  |   English : Alldatasheet.net  |   Chinese : Alldatasheetcn.com  |   German : Alldatasheetde.com  |   Japanese : Alldatasheet.jp
Russian : Alldatasheetru.com  |   Korean : Alldatasheet.co.kr  |   Spanish : Alldatasheet.es  |   French : Alldatasheet.fr  |   Italian : Alldatasheetit.com
Portuguese : Alldatasheetpt.com  |   Polish : Alldatasheet.pl  |   Vietnamese : Alldatasheet.vn
Indian : Alldatasheet.in  |   Mexican : Alldatasheet.com.mx  |   British : Alldatasheet.co.uk  |   New Zealand : Alldatasheet.co.nz
Family Site : ic2ic.com  |   icmetro.com